塑料模具钢材及其处理:
模具钢细节
|
AISI
|
DIN
|
钢材名称
|
初始硬度
|
热处理
|
用途
|
|
1040
|
1.1730
|
ASSAB760
|
13-18HRC
|
/
|
plastic mold base,ejector plate,support pillar,stop pin etc.
|
|
1045
|
K-100
|
|
1050
|
DAIDO P1
|
|
P20
|
1.2738
|
ASSAB 718
|
28-32 HRC
|
/
|
plastic mold cavity and core insert
|
|
1.2311
|
THYSSEN 2311
|
|
|
P20H
|
1.2711
|
ASSAB 718 H
|
35-38 HRC
|
/
|
plastic mold cavity and core block
|
|
THYSSEN 711
|
|
H13
|
1.2344
|
ASSAB 8407
|
190 HB
(12 HRC)
|
48-52 HRC
|
plastic mold cavity and core block ,sprue,slide,ejector pin etc.
|
|
THYSSEN 2344ESR
|
|
o1
|
1.2510
|
ASSAB DF-2
|
180-220 HB
(10-18 HRC)
|
54-56 HRC
|
plastic mold cover plate,insert,gib etc.
|
|
THYSSEN 2510
|
|
S-7
|
1.2767
|
ASSAB S-7
|
200 HB(15 HRC)
|
54-56 HRC
|
impact insert,cover plate,etc
|
|
THYSSEN 2379
|
|
420
|
1.2083
|
STAVAX S-136
|
180-220 HB
(10-18 HRC)
|
Mirrior polishing,HRC 52-54
|
Mirrior polishing steel or PVC plastic
|
|
THYSSEN 2083 ESR
|
PVC plastic,HRC 46-48
|
|
420H
|
1.2316
|
S-136H
|
32-34 HRC
|
/
|
PVC,acidic plastic etc.
|
|
THYSSEN 2316ESR
|
|
|
|
|
210-240 HB(15-22 HRC)
|
HRC 56-60
|
plastic mold core pin,sub gate insert etc.
|
|
BeCu
|
/
|
mold max
|
40-42 HRC
|
/
|
good for cooling
|
|
Al-Bronze
|
/
|
/
|
/
|
/
|
angle lift gib etc
|
塑料产品用料包括:
非工程塑料:PP, HDPE, PS, HIPS
工程塑料:聚碳酸酯,聚酰胺,聚缩醛,聚氧化甲烯树脂,POM/PET,PBT/ABS
耐腐蚀性钢材:S136,2316,420, NAK80等,用于腐蚀性塑料原料
材料:PVC, POM, PC等,模具钢要求透明,高抛光度,镜面效果
塑料:S136, 2316, 718S, NAK80, PAK90, 420
塑料模具钢处理:1. 淬火预处理 2 塑料模具表面硬度的氮化处理,使模具表面硬度达到52-55 HRC,从而在模具碰撞过程中,即使受到磨损或侵蚀,型腔也能够保持灵活自如
|